PENGARUH LAMA CURING DAN VARIASI RASIO Na2SiO3 DENGAN NaOH TERHADAP SIFAT MEKANIK AGREGAT BUATAN GEOPOLYMER BERBASIS FLY-ASH DENGAN METODE CRUSHING

PASARIBU, MUHAMMAD ARIF HUSIN and Adhitya, Bimo Brata and Costa, Anthony (2024) PENGARUH LAMA CURING DAN VARIASI RASIO Na2SiO3 DENGAN NaOH TERHADAP SIFAT MEKANIK AGREGAT BUATAN GEOPOLYMER BERBASIS FLY-ASH DENGAN METODE CRUSHING. Undergraduate thesis, Sriwijaya University.

[thumbnail of RAMA_22201_03011181823007.pdf] Text
RAMA_22201_03011181823007.pdf - Accepted Version
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (4MB) | Request a copy
[thumbnail of RAMA_22201_03011181823007_TURNITIN.pdf] Text
RAMA_22201_03011181823007_TURNITIN.pdf - Accepted Version
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (6MB) | Request a copy
[thumbnail of RAMA_22201_03011181823007_0010038104_0022079003_01_front_ref.pdf] Text
RAMA_22201_03011181823007_0010038104_0022079003_01_front_ref.pdf - Accepted Version
Available under License Creative Commons Public Domain Dedication.

Download (2MB)
[thumbnail of RAMA_22201_03011181823007_0010038104_0022079003_02.pdf] Text
RAMA_22201_03011181823007_0010038104_0022079003_02.pdf - Accepted Version
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (1MB) | Request a copy
[thumbnail of RAMA_22201_03011181823007_0010038104_0022079003_03.pdf] Text
RAMA_22201_03011181823007_0010038104_0022079003_03.pdf - Accepted Version
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (1MB) | Request a copy
[thumbnail of RAMA_22201_03011181823007_0010038104_0022079003_04.pdf] Text
RAMA_22201_03011181823007_0010038104_0022079003_04.pdf - Accepted Version
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (2MB) | Request a copy
[thumbnail of RAMA_22201_03011181823007_0010038104_0022079003_05.pdf] Text
RAMA_22201_03011181823007_0010038104_0022079003_05.pdf - Accepted Version
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (1MB) | Request a copy
[thumbnail of RAMA_22201_03011181823007_0010038104_0022079003_06_ref.pdf] Text
RAMA_22201_03011181823007_0010038104_0022079003_06_ref.pdf - Bibliography
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (1MB) | Request a copy
[thumbnail of RAMA_22201_03011181823007_0010038104_0022079003_07_lamp.pdf] Text
RAMA_22201_03011181823007_0010038104_0022079003_07_lamp.pdf - Accepted Version
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (2MB) | Request a copy

Abstract

Burning coal to produce electrical energy in PLTU produces waste in the form of fly ash. This waste must be managed properly so that it does not cause detrimental environmental impacts. Fly ash has potential as a building material because it contains silica, aluminum, and other oxides which can react with alkaline solutions to form geopolymer compounds. Geopolymer has good mechanical properties and is resistant to acidic and alkaline environments. Development of aggregate materials artificial geopolymer Fly ash-based crushing method becomes an interesting thing. Done Because can utilize fly ash waste and reduce dependence on aggregate nature. Apart from that, this material can also be used to help reduce the impact environment from development construction. The crushing method is used to get aggregate artificial geopolymer with to desired size. Aggregate can be destroyed become more particles small use technique destruction like destroyer mechanical or tools such as Hammer Mill, Jaw Crusher, or Ball Mill. The AIV percentage reached 13.20% at a Na2SiO3/NaOH ratio of 2, however, decreased to 12.64% at a Na2SiO3/NaOH ratio of 3.5. The AIV percentage reached 12.82% without the addition of sand, however, decreased to 12.64% when the addition of sand by 20%. However, the AIV value increased to 12.76% when the addition of sand reached 40%. The AIV percentage reached 12.64% after curing for 24 hours, however, decreased to 12.46% at 48 hours of curing, and AIV increased to 12.94% at 72 hours of curing. Keywords: geopolymer aggregate, crushing, curing time, Na2SiO3 /NaOH, addition sand, aggregate impact value

Item Type: Thesis (Undergraduate)
Uncontrolled Keywords: agregat geopolimer, penghancuran, waktu pemeraman, Na2SiO3/NaOH, penambahan pasir, nilai tumbukan agregat
Subjects: T Technology > TA Engineering (General). Civil engineering (General) > TA165 Engineering instruments, meters, etc. Industrial instrumentation
Divisions: 03-Faculty of Engineering > 22201-Civil Engineering (S1)
Depositing User: Muhammad Arif Husin Pasaribu
Date Deposited: 07 May 2024 00:58
Last Modified: 07 May 2024 00:58
URI: http://repository.unsri.ac.id/id/eprint/143736

Actions (login required)

View Item View Item