SAPUTRA, FANHAR and Nukman, Nukman and Pratiwi, Diah Kusuma (2016) ANALISIS PENGARUH QUENCHING DAN TEMPERING BESERTA VARIASI WAKTU TAHAN DENGAN MEDIA PENDINGIN OLI MESRAN SAE 40 TERHADAP STRUKTUR MIKRO DAN SIFAT MEKANIK BAJA KARBON SEDANG. Undergraduate thesis, University of Sriwijaya.
Preview |
Text
RAMA_21101_03111005064 _ 0021035910_0019076305 _01_front_ref.pdf - Accepted Version Available under License Creative Commons Public Domain Dedication. Download (212kB) | Preview |
Text
RAMA_21101_03111005064 _ 0021035910_0019076305 _02.pdf - Accepted Version Restricted to Repository staff only Available under License Creative Commons Public Domain Dedication. Download (439kB) | Request a copy |
|
Text
RAMA_21101_03111005064 _ 0021035910_0019076305 _03.pdf - Accepted Version Restricted to Repository staff only Available under License Creative Commons Public Domain Dedication. Download (424kB) | Request a copy |
|
Text
RAMA_21101_03111005064 _ 0021035910_0019076305 _04.pdf - Accepted Version Restricted to Repository staff only Available under License Creative Commons Public Domain Dedication. Download (730kB) | Request a copy |
|
Text
RAMA_21101_03111005064 _ 0021035910_0019076305 _05_ref.pdf - Bibliography Restricted to Repository staff only Available under License Creative Commons Public Domain Dedication. Download (11kB) | Request a copy |
|
Text
RAMA_21101_03111005064 _ 0021035910_0019076305 _06_lamp.pdf - Accepted Version Restricted to Repository staff only Available under License Creative Commons Public Domain Dedication. Download (420kB) | Request a copy |
Abstract
The purpose of this research is to compare the mechanical properties and micro structure of the medium carbon steel, with heat treatment or without heat treatment. The heat treatments used are quench and quench-temper. The results of this research are the highest impact energy is on quenching 60 minutes – temper material which the increased is 16,39 % compare to non-heat treatment material, while the lowest impact energy is on quenched 30 minutes and its decreased 58,55 % compare to non-heat treatment. For the hardness value, the highest one is on quenched 30 minutes material which is increased to 30,69 % compare to raw material. Whereas the highest value of the tensile strength is on quenched 30 minutes, which is increased to 39,84 % compare to raw material and for the highest fracture value is also on quenched 30 minutes, and its increased to 32,01 % compare to non-heat treatment material, and the highest value of strain is on quenched 60 minutes – temper material, its increased to 6,42 % compare to the non-heat treatment. Then almost every materials or specimens on this research have ferrite and pearlite as its microstructure as well.
Item Type: | Thesis (Undergraduate) |
---|---|
Uncontrolled Keywords: | medium carbon steel, quenching, non-heat treatment, tempering, Mesran SAE 40 oil, impact testing, hardness testing, tensile testing, microstructure |
Subjects: | T Technology > TJ Mechanical engineering and machinery > TJ1-1570 Mechanical engineering and machinery |
Divisions: | 03-Faculty of Engineering > 21101-Mechanical Engineering (S2) |
Depositing User: | Mrs. Elly Suryani |
Date Deposited: | 21 Nov 2019 04:06 |
Last Modified: | 21 Nov 2019 04:06 |
URI: | http://repository.unsri.ac.id/id/eprint/17514 |