PENGARUH VARIASI SERBUK BOTOL KACA SEBAGAI SUBSTITUSI SEMEN PADA SELF COMPACTING CONCRETE (SCC) TANPA PERAWATAN

MAHANI, INDRI and Rosidawani, Rosidawani (2019) PENGARUH VARIASI SERBUK BOTOL KACA SEBAGAI SUBSTITUSI SEMEN PADA SELF COMPACTING CONCRETE (SCC) TANPA PERAWATAN. Undergraduate thesis, Sriwijaya University.

[thumbnail of RAMA_22201_03011181419074.pdf] Text
RAMA_22201_03011181419074.pdf - Accepted Version
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (5MB) | Request a copy
[thumbnail of RAMA_22201_03011181419074_turnitin.pdf] Text
RAMA_22201_03011181419074_turnitin.pdf - Accepted Version
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (11MB) | Request a copy
[thumbnail of RAMA_22201_03011181419074_000905601_01_front_ref.pdf]
Preview
Text
RAMA_22201_03011181419074_000905601_01_front_ref.pdf - Accepted Version
Available under License Creative Commons Public Domain Dedication.

Download (618kB) | Preview
[thumbnail of RAMA_22201_03011181419074_000905601_02.pdf] Text
RAMA_22201_03011181419074_000905601_02.pdf - Accepted Version
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (456kB) | Request a copy
[thumbnail of RAMA_22201_03011181419074_000905601_03.pdf] Text
RAMA_22201_03011181419074_000905601_03.pdf - Accepted Version
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (138kB) | Request a copy
[thumbnail of RAMA_22201_03011181419074_000905601_04.pdf] Text
RAMA_22201_03011181419074_000905601_04.pdf - Accepted Version
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (446kB) | Request a copy
[thumbnail of RAMA_22201_03011181419074_000905601_05.pdf] Text
RAMA_22201_03011181419074_000905601_05.pdf - Accepted Version
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (132kB) | Request a copy
[thumbnail of RAMA_22201_03011181419074_000905601_06_ref.pdf] Text
RAMA_22201_03011181419074_000905601_06_ref.pdf - Bibliography
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (62kB) | Request a copy
[thumbnail of RAMA_22201_03011181419074_000905601_07_lamp.pdf] Text
RAMA_22201_03011181419074_000905601_07_lamp.pdf - Accepted Version
Restricted to Repository staff only
Available under License Creative Commons Public Domain Dedication.

Download (1MB) | Request a copy

Abstract

Self compacting concrete or called SCC is a concrete innovation to overcome the solution of difficult casting and compacting processes, especially concrete with complex reinforcement. The SCC composition uses a considerable amount of cement compared to conventional concrete in order to achieve the required flow, so there needs to be a substitution to reduce it. The SCC composition uses a considerable amount of cement, so there is a need for substitution to reduce it. With that condition, the research on SCC has evolved to reduce cement. One of them is the using of waste glass as a substitution. SCC is affected by the process of casting and curing, but in the actual condition it is usually neglected. This study was conducted to determine the effect of glass bottle powder as cement substitution on the characteristics of SCC workability and concrete compressive strength without curing. The variation of glass bottle powder use are 0%, 2.5%; 7.5%; 12.5%; and 17.5%. The results of fresh concrete test indicate that the using of glass bottle powder can decrease SCC workability, but still on the requirements. The result of the slump flow test on the highest glass percentage SCC-1 (2,5%) is decreased to 2,9% with a slump flow of 670 mm, the results of the V-Funnel test on the highest percentage of glass bottle powder SCC-1 (2,5%) isdecreased to 3.88% with 10.7 secondsflow time, and the L-Box test results on the highest percentage of glass bottle powder SCC-1 (2,5%) isdecreased to 1.15% with 0.86H2/H1 ratio. these decreases occur because the shape of glass bottles are angular shape, thereby reducing work ability. The compressive strength test results show increases up to 7,5% variation ofsubstitution of bottle powder variation on SCC-3 with compressive strength reach 55.11 Mpa or 17,65% more than SCC-0.

Item Type: Thesis (Undergraduate)
Uncontrolled Keywords: SCC, Serbuk Botol Kaca, Non Curing, Slump Flow, Workability
Subjects: T Technology > TA Engineering (General). Civil engineering (General) > TA630-695 Structural engineering (General)
Divisions: 03-Faculty of Engineering > 22201-Civil Engineering (S1)
Depositing User: Users 1210 not found.
Date Deposited: 08 Aug 2019 06:43
Last Modified: 08 Aug 2019 06:43
URI: http://repository.unsri.ac.id/id/eprint/3016

Actions (login required)

View Item View Item